| 73 | 0 | 53 |
| 下载次数 | 被引频次 | 阅读次数 |
为探究不同养护制度、成型工艺及纳米SiO2掺量对超高韧性混凝土(STC, Super Toughness Concrete)断裂性能的影响,本文采用三点弯曲切口梁试验,研究了在两种养护制度(蒸汽养护、自然养护)及两种成型工艺(薄层夯捣、常规浇筑)下STC的断裂特性。结果表明:薄层夯捣下,2%纳米SiO2掺量的混凝土试件极值荷载最高,常规工艺下不掺纳米SiO2时最高;薄层夯捣下混凝土的断裂能整体大于常规工艺,随纳米SiO2掺量的增加先增大后减小,且两种养护制度下断裂能相差较小;两种养护制度下,薄层夯捣后的混凝土起裂韧度和失稳韧度整体均高于常规工艺;各工况断裂过程区最大长度均在67 mm左右。
Abstract:In order to explore the effects of molding process and nano-SiO2 on the fracture properties of Super Toughness Concrete (STC) under different curing regimes, three-point bending beam test was adopted to study the effects of different curing systems (steam curing, natural curing) and two molding processes (thin-layer tamping, conventional process) on the fracture properties of STC. The results show that: under thin-layer tamping, the extreme load of concrete specimens with 2% nano-SiO2 is the highest, and that without nano-SiO2 is the highest under the conventional process; the fracture energy of concrete under thin-layer tamping is larger than that under the conventional process, and it increases firstly and then decreases with the increase of nano-SiO2, and the difference of fracture energy between two kinds of curing regimes is relatively small; the initiation toughness and instability toughness of the concrete under the two curing regimes are both greater than that under the conventional process; the maximum length of the fracture process area of the various conditions is about 67 mm.
[1] 陈聪聪,吴泽媚,胡翔等.钢纤维形状和养护制度对超高性能混凝土强度及韧性的影响[J].材料导报,2024,38(15):139-149.
[2] 李林香,谭盐宾,杨鲁,等.纳米SiO_(2)对C60高强混凝土性能的影响[J].铁道建筑,2025,65(10):154-159.
[3] Hosan A, Shaikh F, Sarker P, et al. Nano- and Micro-scale Characterisation of Interfacial Transition Zone (ITZ) of High-volume Slag and Slag-fly Ash Blended Concretes Containing Nano-SiO_(2) and Nano-CaCO_(3) [J]. Construction and Building Materials, 2020, 269(5):121311.
[4] Huang H, Gao X, Khayat K H. Contribution of Fiber Alignment on Flexural Properties of UHPC and Prediction Using the Composite Theory[J]. Cement and Concrete Composites, 2021(7):103971.
[5] 张冲, 毕梦迪, 刘同军等.砂浆流变性能和外界磁场强度对钢纤维分布特征的影响[J].材料导报,2022, 36(24):74-79.
[6] Xu S, Reinhardt H W. Determination of Double-K Criterion for Crack Propagation in Quasi-brittle Fracture, Part I: Experimental Investigation of Crack Propagation[J]. International Journal of Fracture, 1999, 98(2):111-149.
[7] Xu S, Reinhardt H W. Crack Extension Resistance and Fracture Properties of Quasi-brittle Softening Materials like Concrete Based on the Complete Process of Fracture[J]. International Journal of Fracture, 1998, 92(1):71-99.
[8] Reinhardt H W, Xu S. Crack Extension Resistance Based on the Cohesive Force in Concrete[J]. Engineering Fracture Mechanics, 1999, 64(5):563-587.
[9] Jenq Y, Shah S P. Two Parameter Fracture Model for Concrete[J]. Journal of Engineering Mechanics, 1985, 111(10):1227-1241.
[10] Wecharatana M, Shah S P. Predictions of Nonlinear Fracture Process Zone in Concrete[J]. Journal of Engineering Mechanics, 1983, 109(5):1231-1246.
基本信息:
中图分类号:TU528
引用信息:
[1]万美萱,曾慧姣,李玉鹏,等.不同养护制度和成型工艺下STC断裂性能[J].铁道建筑().
基金信息:
国家自然科学基金(52278277)