| 48 | 0 | 80 |
| 下载次数 | 被引频次 | 阅读次数 |
针对朔黄重载铁路换铺无缝线路时U78CrVH钢轨焊接接头出现的伤损问题,通过宏观形貌观察、扫描电镜(SEM)、能谱分析(EDS)、金相检验、化学成分检测等手段进行系统分析。结果表明:钢轨轧制形成的带状组织使非金属夹杂物沿轧向层状分布;焊接顶锻后推凸装置横向切除凸起时,焊缝区承受垂直剪切应力,当应力超过带状组织强度时,裂纹优先在MnS等夹杂物处萌生。伤损位于轨腰次表面,呈熔融形貌,含Mn、S等元素富集,判定为推凸裂纹。建议提高钢轨母材纯净度,放宽推凸尺寸并增加余高,以预防此类裂纹。
Abstract:Aiming at the damage occurring in U78CrVH rail welded joints during the relaying of continuous welded rail on the Shuohuang heavy-haul railway, a systematic analysis was conducted by means of macroscopic morphology observation, scanning electron microscopy (SEM), energy dispersive spectroscopy (EDS), metallographic examination, and chemical composition analysis. The results show that the banded structure formed during rail rolling causes non-metallic inclusions to distribute in layers along the rolling direction. When the trimming device transversely removes the protrusion after welding upsetting, the weld zone is subjected to vertical shear stress. Once the stress exceeds the strength of the banded structure, cracks preferentially initiate at inclusions such as MnS. The damage is located at the subsurface of the rail web, exhibiting a molten morphology with enrichment of elements such as Mn and S, and is thus identified as a trimming crack. It is recommended to improve the cleanliness of the rail base metal, relax the trimming dimension, and increase the weld reinforcement, so as to prevent such cracks.
[1]凌烈鹏,王新让,周游,等.朔黄铁路线路设备状态检测模式分析[J].铁道建筑,2019,59(10):127-131.
[2]刘嘉,杨相健,罗世辉,等.朔黄铁路重载列车线路适应性仿真研究[J].振动、测试与诊断,2020,40(4):673-821.
[3]刘光鹏,肖宏,王宏阁,等.重载铁路钢轨隐伤病害处振动特性分析[J].振动与冲击,2022,41(3):245-252.
[4]何庆,杨康华,杨翠平,等.铁路曲线地段钢轨生存寿命评估与分析[J].铁道科学与工程学报,2021,18(8):2038-2046.
[5]丁韦,张宪良,赵国,等.钢轨闪光焊推凸缺陷的形成及预防对策[J].铁路技术创新,2016,(02):55-57.
[6]丁韦,高文会,宋宏图,等.U75V钢轨闪光焊推凸引致裂纹的分析[J].理化检验(物理分册),2005,41(增刊1):537-539.
基本信息:
中图分类号:U213.92;U239.4
引用信息:
[1]尹段泉.朔黄重载铁路无缝线路钢轨焊接接头伤损分析[J].铁道建筑().
基金信息:
国家能源投资集团有限责任公司技术开发课题(GJNY-25-94)
2026-09-14
2026-09-14
2026-09-14